navitron
 
Renewable Energy and Sustainability Forum
UK's most popular Renewable Energy Forum May 24, 2012, 11:27:48 AM *
Welcome, Guest. Please login or register.

Login with username, password and session length
News: Anyone wishing to register as a new member on the forum is strongly recommended to use a "proper" email address - following recent spam/hack attempts on the forum, all security is set to "high", and "disposable" email addresses like Gmail, Yahoo and Hotmail tend to be viewed with suspicion, and the application rejected if there is any doubt whatsoever
 
Recent Articles: UPDATE ON DECC APPLICATION FOR LEAVE TO APPEAL TO THE SUPREME COURT | Yingli Green Energy's PV Module Ranks No.2 in TUV Rheinland Energy Yield Test | Navitron Solar Showers at Glastonbury for Year 5!
   Home   Help Search Login Register  
Pages: [1]   Go Down
  Print  
Author Topic: High Temperature Adhesive  (Read 539 times)
Tigger
Sr. Member
****
Offline Offline

Posts: 301


« on: August 15, 2011, 10:33:50 AM »

Folks,

I need to repair the plastic lid of a steamer, standard epoxy resins only go up to 65 - 70'C and whilst I know the lid of the steamer probably won't hit 100'C, I'm not convinced it would be long before it gave in and it would also exclude it from being put in the dishwasher.

I had a trawl on t'internet for high temp plastic adhesive and then a search on this wonderful forum for the same and didn't really get anywhere.  Bond-IT 7050 (from the USA) was all the great WWW could come up with and I can't find a UK seller and there was nothing on here that I could find.  I've also got to bear in mind that I might be able to buy a new lid cheaper than buying a specialist adhesive.

So.......

Anybody out there got any ideas?Huh

Thanks,

Ian.



Logged

30 tubes, south facing gable wall (Navitron Fornax Trial System).  Hunter Herald 8, integrated boiler hooked up with Oil Boiler via Dunsley Neutraliser.  Scrounging fire wood wherever possible Smiley
djh
Hero Member
*****
Offline Offline

Posts: 1222


« Reply #1 on: August 15, 2011, 11:31:09 AM »

There are high temperature cyanoacrylates, e.g. http://www.permabondllc.com/TDS/801_TDS.pdf

You could also try calling an adhesives manufacturer.
Logged

Cheers, Dave
Tigger
Sr. Member
****
Offline Offline

Posts: 301


« Reply #2 on: August 15, 2011, 11:52:52 AM »

Thanks djh, as usual my web trawling was not up to scratch.

I found a UK supply of Permabond 801 but sadly a small bottle (20g) will cost me £23.44 and I could buy a new steamer for £20 which just reinforces my worry that buying a new lid (or steamer) will be cheaper than the repair.

I know I could buy it knowing I'll find another use but with a shelf life of only 12 months, I'm pushing my luck.

I'll get in touch with Permabond and see what they say.

Thanks,

Ian.

Logged

30 tubes, south facing gable wall (Navitron Fornax Trial System).  Hunter Herald 8, integrated boiler hooked up with Oil Boiler via Dunsley Neutraliser.  Scrounging fire wood wherever possible Smiley
Ivan
Administrator
Hero Member
*****
Offline Offline

Posts: 1221


« Reply #3 on: August 17, 2011, 12:24:49 AM »

Why not use standard silicone. Silicone sealant was invented primarily as a bonding agent, but then found popularity as a sealant. It's good for 200C.
Logged

Navitron Member of Staff
www.epogee.co.uk - Solar PV & Solar Thermal Training / MCS
Tigger
Sr. Member
****
Offline Offline

Posts: 301


« Reply #4 on: August 17, 2011, 10:11:51 AM »

Agh, I gave in last night and went for standard epoxy in the hope that the lid will never get too hot Sad


Thanks anyway Ivan, if the epoxy resin fails then I'll do my best to clean it off and try the silicon sealant instead Smiley
Logged

30 tubes, south facing gable wall (Navitron Fornax Trial System).  Hunter Herald 8, integrated boiler hooked up with Oil Boiler via Dunsley Neutraliser.  Scrounging fire wood wherever possible Smiley